Forming a Round Wound Core into a Rectangle: Where Does Strain Accumulate?

  • Chenfan Power

Track each sheet through round-to-rectangle forming: curvature changes, same-sheet strain and interlayer slip. Inspect the corner apexes, tangent transitions and unbending straight sections against tool contact and restraint through the stroke. This locates the mechanism behind a strained or displaced layer.

Calculation basis. Numerical demonstrations use editorial assumptions unless a value is expressly attributed to a cited supplier, standard or published study. Dimensions describe the stated model geometry; test results introduced with “assume” or “suppose” are hypothetical inputs. Calculated outputs inherit those conditions.

Follow the sheet through the forming path

For a circular starting layer, curvature is distributed around the perimeter. In a rounded rectangular finish, most turning occurs at four corners; straight sections have approximately zero in-plane curvature. Material that becomes a straight section has undergone unbending. It should not be classified as untouched simply because it looks straight afterward.

The corner apex is a candidate for substantial bending strain, particularly where the radius becomes small. The tangent regions on either side also deserve attention: the curvature changes there, and tool contact can change while the layer is still moving. If a layer is restrained by friction or a clamp, additional longitudinal strain can appear away from the smallest radius. The actual peak location depends on the forming sequence, contact conditions and layer constraints; it cannot be established from the final outline alone.

In the forming route considered here, a cylindrical laminated body is reshaped into a rectangle. Track each layer because its corner radius, contact and material movement can differ through the build.

Separate interlayer movement from material extension

Place two identifiable marks on the same sheet and follow their material separation. Use a separate pair of marks on neighbouring sheets to observe relative movement. These are different measurements.

For a same-sheet gauge, engineering strain is ε = (ℓ − ℓ₀)/ℓ₀, where ℓ₀ and ℓ are the initial and current lengths along the tracked material line, in the same units. Choose the strain measure consistently if deformation is large. A sheet moving around the perimeter without changing this material length has displacement, but no extension of that line.

For two adjacent sheets, relative tangential movement is Δu_rel = Δu₁ − Δu₂, measured against a common datum and with the local tangential direction defined. A change in this value indicates interlayer slip at the observed location. It does not, by itself, establish either sheet’s longitudinal strain. Slip and stretching can occur together.

In the elementary thin-beam approximation, longitudinal surface strain contains middle-line extension plus a through-thickness bending term. Use paired surface and curvature evidence to separate those quantities.

Conceptual round-to-rectangle wound-core forming path showing corner and tangent inspection zones, same-sheet material gauges and adjacent-layer slip measurements
Round-to-rectangle forming path and separate measurements for material extension and interlayer slip. Highlighted zones are inspection candidates, not measured strain contours. Conceptual diagram — not a manufacturing drawing.

A chord-length trap that can mimic strain

Assumed calculation inputs and results. Consider an ideal inextensible material line with a 20.000 mm gauge length. Assume it first follows a circular arc of radius 100.000 mm, then becomes straight or follows an arc of radius 20.000 mm. This isolates geometry; it is not a finite-thickness steel-sheet model.

For an arc length ℓ and radius R, the endpoint chord is c = 2R sin[ℓ/(2R)], with the angle in radians. Initially c₀ = 19.9667 mm. The straight-line chord becomes 20.0000 mm, while the tighter-arc chord becomes 19.1770 mm. Comparing chords would suggest +0.1669% extension or −3.9549% contraction. The assumed material-line length is unchanged, so its actual extension is zero.

The practical lesson is to reconstruct the tracked material length or use a validated local strain calculation. Two-point image distance in a fixed view is insufficient when curvature or orientation changes. This geometric error is separate from camera perspective error and from real surface strain caused by bending.

Specify measurement zones before the trial

Use a stable core coordinate system and retain material-point identities as the shape changes. The following matrix defines a diagnostic study, not universal acceptance limits.

ZoneObservationDecision it supports
Apex of each of the four cornersLocal shape and same-sheet strain through the strokeWhether bending-related response is symmetric or concentrated in one corner
Both tangent transitions at each cornerCurvature profile and local strain, with tool-contact timingWhether the strongest response occurs at the transition rather than the apex
Midpoint of every future straight sideSame-sheet material length and curvatureWhether unbending is accompanied by longitudinal extension
Accessible inner, middle and outer layer positionsLayer identity, local radius and paired relative displacementWhether the observed motion varies through the build
Joint region, where present, and restrained contact zonesEnd movement, overlap change and local strainWhether closure movement or restraint explains an apparent extension

Middle layers are frequently hidden. Exposed-edge marks can establish relative motion where they are visible, but do not reveal a complete buried-layer strain field. A dedicated development specimen or a separately validated model may be needed. Record which layers and faces were actually observed; do not label an outer-face map as a whole-core map.

Capture the sequence, including unloading

Record the circular reference state, intermediate forming states, the final loaded state and the unloaded state before any later thermal treatment. Synchronize observations with tool displacement, force and contact changes. Comparing only the first and last images loses information about slip onset and temporary strain maxima. Comparing loaded and unloaded states helps distinguish reversible shape change from retained deformation, but retained surface strain alone is not a complete residual-stress measurement.

Digital image correlation (DIC) can help, provided the measurement is designed for the motion. The iDICs Good Practices Guide, Edition 2 (2025), explains that out-of-plane movement can create false strain in single-camera 2D-DIC. Use stereo-DIC where appropriate, or quantify the error of the selected arrangement. Establish a no-deformation noise baseline and check rigid-body movement. Test the virtual strain-gauge size: excessive spatial averaging can conceal a narrow peak. Process each sheet’s observed region separately so that averaging does not bridge a slipping interface. [2]

Decide what the evidence can establish

A forming study should report where curvature changes, where same-sheet strain develops, where relative layer movement begins, and which effects persist after unloading. Agreement between these observations is more useful than a single maximum-strain number.

Set acceptance criteria using the actual steel grade, coating, thickness, joint design and qualified forming route. Qualify the specified geometry on that basis, then verify magnetic performance with controlled loss and excitation tests.

Calculate the bending component before interpreting surface strain

Nippon Steel lists 23ZH90 at a nominal steel thickness of 0.23 mm and an assumed density of 7.65 kg/dm³. [1] In a separate elementary thin-sheet screen, assume the neutral line is at the sheet mid-thickness and follows a 20.0 mm radius. Surface bending-strain magnitude is t/(2R) = 0.23/(2 × 20) = 0.00575, or 0.575%. At an assumed 100 mm radius it is 0.115%, five times smaller. Opposite faces have opposite bending signs in this model. Measure the actual curvature and same-sheet material length to distinguish bending from middle-line extension. [2]

Manufacturing controls. Control layer radius, tool contact, winding tension, restraint, interlayer slip and the unloading history. Match surface-pattern motion to the sheet beneath it and assess out-of-plane optical error before interpreting a strain peak.

References

[1] Nippon Steel Corporation, Grain-Oriented Electrical Steel Sheets, undated, specification tables and annealing compatibility.

[2] E. M. C. Jones and M. A. Iadicola (eds.), A Good Practices Guide for Digital Image Correlation, Edition 2, 2025, DOI 10.32720/idics/gpg.ed2.

Chenfan Electric

Direct coordination