| Metric | Test point | Value | Source |
|---|---|---|---|
| Specific core loss | 50 Hz · 1.7 T (B) | 0.95 W/kgGuaranteed maximum | PDF page 5 |
| Specific core loss | 50 Hz · 1.5 T (B) | 0.71 W/kgTypical | PDF page 6 |
| Specific core loss | 50 Hz · 1.7 T (B) | 0.94 W/kgTypical | PDF page 6 |
| Specific core loss | 60 Hz · 1.5 T (B) | 0.94 W/kgTypical | PDF page 6 |
| Specific core loss | 60 Hz · 1.7 T (B) | 1.24 W/kgTypical | PDF page 6 |
| Magnetic induction | 800 A/m | 1.88 TGuaranteed minimum | PDF page 5 |
| Magnetic induction | 800 A/m | 1.91 TTypical | PDF page 6 |
| Magnetic induction | 2500 A/m | 1.96 TTypical | PDF page 6 |