A defect recorded 318.4 m from a parent coil’s reference end needs a coordinate map before 318.4 m can be interpreted in a daughter’s payout frame. Splitting changes the origin; reversing material order changes the sign. Keep those transformations with the coil genealogy.
Calculation basis. Numerical demonstrations use editorial assumptions unless a value is expressly attributed to a cited supplier, standard or published study. Dimensions describe the stated model geometry; test results introduced with “assume” or “suppose” are hypothetical inputs. Calculated outputs inherit those conditions.
The useful planning record keeps a material-based parent coordinate and an explicit map to each daughter’s working coordinate. Use the derived map for a length-preserving split and include the stated position-error allowance. Set the defect class and discard interval from the approved material requirements.
Define the parent coordinate independently of the machine counter
Choose a documented physical reference end for the parent coordinate x, state its positive direction and use consistent units. Record defect extent as an interval [d1,d2], rather than reducing every defect to one center point. Keep the observed material face and transverse position where those affect the disposition.
A usable defect map preserves observed defect extent, material identity, longitudinal reference, transverse position and the evidence behind each coordinate. Validate its physical registration before using the map to exclude material from a cutting plan.
A machine counter is a measurement of a process coordinate. Its reset, scale, reference mark and relationship to the parent material coordinate must be recorded. “The counter started at zero” leaves open which physical end was present and whether it measured the retained segment, a trimmed head or material passing a different reference station.
Give every daughter an origin and a sign
Let a daughter retain the parent interval [a,b], with ideal retained length L = b − a. Define its working coordinate s from the end that will serve as its documented zero. If parent material order is preserved, use:
s = x − a; inverse: x = a + s
If the working order is reversed, use:
s = b − x; inverse: x = b − s
These are affine maps with slope +1 or −1. A reversing operation should not be inferred merely from the word “rewound”; confirm which parent end becomes the working zero after the actual handling sequence. Material-face and transverse-direction changes require their own records and are not resolved by the longitudinal sign alone.
Clip a defect to the retained parent interval before transforming it. If its intersection is [u,v], the forward interval is [u−a,v−a], while the reversed interval is [b−v,b−u]. Reversing the endpoints without sorting would produce a negative-width interval. If there is no intersection, that particular daughter does not contain the recorded defect interval.
For a defect crossing a split, preserve the clipped portion on each affected daughter and retain the common parent event identity. Do not drop an event just because its center lies outside one daughter. An exact split-end boundary also needs a documented ownership convention for records and allowances.

An independently reversible example
Assume a daughter retains parent x = 200.0–500.0 m, giving L = 300.0 m. The parent defect interval is x = 318.4–319.1 m. Assume ideal preserved length and no material removal within that segment.
| Working order | Coordinate rule | Daughter defect interval | Inverse check |
|---|---|---|---|
| Forward | s = x − 200.0 | 118.4–119.1 m | 200.0 + endpoints = 318.4–319.1 m |
| Reversed | s = 500.0 − x | 180.9–181.6 m | 500.0 − endpoints, reordered = 318.4–319.1 m |
Both intervals have width 0.7 m, as does the parent interval. Their positions differ because their zeros lie at opposite parent ends. A cut-to-length program using 118.4–119.1 m for the reversed daughter would target the wrong material location despite carrying the correct parent identity.
If a head is subsequently removed, update the retained parent endpoint and the working zero. If material is removed from the interior and the remaining portions are joined, a single affine map is insufficient: use separate retained parent segments with a piecewise working-coordinate map and preserve the discontinuity. The discarded length must not silently remain in the daughter’s counter coordinate.
Carry positional error into the avoidance interval
Coordinate transformation is exact only under its declared assumptions. Position evidence still depends on defect-location measurement, split-end reference and subsequent payout measurement. Separate a sign or reference mistake from small bounded measurement errors: increasing a margin cannot reliably repair an unknown origin.
For an illustrative worst-case allowance, assume maximum absolute endpoint errors of 0.05 m for parent defect location, 0.08 m for the relevant daughter reference endpoint and 0.03 m for subsequent payout registration. These are assumed bounded errors, not standard uncertainties or equipment specifications.
Their conservative sum is 0.16 m. Applying it to the reversed nominal interval gives an illustrative exclusion interval of 180.74–181.76 m. Its width is 1.02 m: the nominal 0.70 m plus 0.16 m at each end. No statistical independence is needed for this worst-case sum; a root-sum-square interpretation would require a different stated uncertainty model.
Set the actual avoidance interval from the approved defect disposition, measured position bounds, processing allowances and decision rule. The 0.16 m teaching allowance illustrates the arithmetic; use the qualified inputs for the material and line in service.
Verify the map before using the cutting plan
Retain parent and daughter identities, retained endpoints, coordinate units, working-end identity, direction sign, removal history and the source of position measurements. Store the original defect interval as well as the transformed planning interval; overwriting the parent coordinate makes later reversal checks difficult.
Test the conversion with known reference positions or qualified checks, including the daughter endpoints and an interior location. Confirm that forward and inverse conversions return the same parent event within the stated numerical and measurement basis.
A usable cutting record locates the same material feature after each split or reversal and carries a stated position bound. Keep that evidence with the cutting decision so production can identify the intended material interval from the daughter’s working end.
Carry the coordinate margin into the scrap balance
Nippon Steel lists 23ZH90 at a nominal steel thickness of 0.23 mm and an assumed density of 7.65 kg/dm³. [1] With an assumed strip width of 300 mm, the 0.70 m nominal defect interval contains 0.369495 kg of nominal steel. The 1.02 m expanded reversed-coordinate interval contains 0.538407 kg. The 0.168912 kg difference is the material reserved for the two 0.16 m position bounds. Verify the transformed endpoints and preserve that disposition after every split; keeping only the nominal defect length loses the avoidance margin.
Manufacturing controls. Control parent origin, daughter endpoint identity, working direction, removed lengths and payout registration. Keep material face and transverse location when either changes which laminations must be rejected.
IEC 60404-8-7 covers supplied grain-oriented electrical-steel magnetic and geometric characteristics. Carry the approved supplied grade and dimensional basis into this manufacturing record. [2]
References
[1] Nippon Steel Corporation, Grain-Oriented Electrical Steel Sheets, undated, specification tables and annealing compatibility.
[2] IEC, IEC 60404-8-7:2020, Magnetic materials — Part 8-7: Specifications for individual materials — Cold-rolled grain-oriented electrical steel strip and sheet delivered in the fully-processed state.