Chenfan Electric
AR
أرسل الرسم
العودة إلى الفيديوهات الهندسية

مكتبة الفيديوهات التقنية

Lamination Cleanliness and Interlaminar Short-Circuit Risk

المدة 00:53 · 1080 × 1920

ملخص تقني

Debris between core laminations can affect insulation, sheet spacing and pressure distribution. This video follows metallic chips and non-metallic contamination through packet building and stacking. It covers separation from cutting and grinding, clean handling, surface inspection and investigation of low core-to-clamp insulation readings.

تنزيل الترجمة النصية

النص الكامل للفيديو
A clean-looking core can still hide something between its sheets. At the cutting line, remove chips and fines before forming packets. A conductive chip can bridge the coating. Contacts that close a loop linked by changing magnetic flux can allow current to circulate across sheets. Non-metallic debris can also hold sheets apart and make pressure uneven. Separate stacking from cutting and grinding. Wear clean gloves, keep tools and packaging off the stack, and inspect the surface before adding the next packet. After assembly, check core-to-clamp insulation resistance. If the reading is low, investigate the cause. The finished core's outside appearance is not a substitute for a clean build.

استفسار عن مشروع

تواصل مع فريقنا ↗
Chenfan Electric

تنسيق مباشر

ابدأ التواصل.

رسم أو متطلب مادة أو مشروع ترغب في مناقشته.

أرسل الرسم