Qualify the wound-core tail fixing for both retention and electrical separation. Trace the contacts created by the tail, bond or band and closure, then evaluate the changing flux linked by any completed conductive path.
Calculation basis. Numerical demonstrations use editorial assumptions unless a value is expressly attributed to a cited supplier, standard or published study. Dimensions describe the stated model geometry; test results introduced with “assume” or “suppose” are hypothetical inputs. Calculated outputs inherit those conditions.
Review the complete path formed by the tail, underlying steel, adhesive or band, clasp and any nearby metal. Then ask what changing magnetic flux threads that path. Electrical closure and magnetic flux linkage must both be understood. Calling every visible metal ring a shorted turn is as misleading as accepting every nonmetallic-looking fixing as insulation.
Map the tail overlap as an electrical assembly
A tail can overlap an earlier layer of the strip. The drawing should identify coated faces, exposed edges, intentional contacts and possible contacts created by pressure or damage. Show the complete steel-strip connectivity, not just the small region visible from outside.
One illustrative local fault is two conductive bridges between the tail and an underlying lamination, separated across the strip width. Current can travel across one steel layer, cross at one bridge, return across the other layer and close at the second bridge. That loop encloses a cross-sectional area that may be threaded by the along-strip working flux. A continuous weld seam can contain multiple such crossing points.
Two local bridges are an example, not a universal minimum fault count. Wound strip is already a continuous conductor along its length, and remote contacts can provide a return path. A single new contact must be assessed against that existing network before it can be declared harmless.
Electrically insulating the steel layers interrupts cross-layer conducting paths. Inspect any new contact in relation to the existing metallic path and its linked flux before classifying the tail fixing. [2]

Check linkage before using a shorted-turn argument
For a stationary closed contour C, Faraday’s law gives:
e(t) = −dΦlinked/dt; Φlinked = ∫S B · n dA
For a closed conducting contour C, Faraday’s law relates induced voltage to the rate of change of magnetic flux through a surface bounded by that contour. Identify the actual linked component before using a shorted-turn model.
A conductive fixing that passes through the core window and closes around a limb can link the main core flux. A ring following the core’s planar outside perimeter does not automatically have that same linkage: the dominant working flux may run along, rather than through, the surface it encloses. Local leakage, fringing and interlaminar paths can still matter. The actual three-dimensional geometry must decide the classification.
For prescribed sinusoidal linked flux with peak value Φpk:
Erms = 2πfΦpk/√2 ≈ 4.443fΦpk
If B is uniform and normal to the chosen area, Φpk = BpkAlinked. Otherwise, integrate the field instead of substituting a gross core area.
Assumed calculation inputs and results. At f = 50 Hz and prescribed Bpk = 1.5 T, a loop linking Alinked = 5 mm² has Φpk = 7.5 µWb and Erms = 1.67 mV. A loop linking 4,000 mm² has Φpk = 6 mWb and Erms = 1.33 V. The area ratio is 800, so the induced-voltage ratio is also 800 under these assumptions.
These examples compare linkage only. They do not assign an actual fault area to a tail joint or predict current, temperature or loss. Those additionally depend on circuit impedance, field redistribution and the excitation source. Do not substitute a resistance measured somewhere else into the example and present the result as a product fault prediction.
Choose a fixing method by its complete material system
A dielectric bond can transfer mechanical load while maintaining intended electrical separation. Specify cured electrical properties, filler system and bondline process; the generic word epoxy does not define conductivity.
For a tail bond, qualify adhesion to the actual coated surface, cure state, bond geometry, retention and electrical separation after the relevant thermal and environmental exposure. A strong bond to a laboratory metal coupon does not prove retention on the selected GO coating. Nor does good initial insulation prove performance after cracking, contamination or displacement.
Insulating tape or glass-fiber restraint provides another mechanical route, but the complete assembly includes resin or adhesive, overlap, fastener and any clasp. A metal closure can reintroduce the path that an insulating band was intended to avoid. Band tension can also change tail seating and pressure; electrical acceptability does not establish the mechanical setting.
| Fixing approach | Electrical question | Mechanical/process question |
|---|---|---|
| Qualified dielectric adhesive | Does the cured bond preserve the intended separation? | Does the coated-surface bond retain the tail through its required exposure? |
| Insulating tape or fiber restraint | Are the backing, binder and closure insulating in the actual assembly? | Does the restraint maintain position without harmful local loading? |
| Metallic clip, seam or band | What cycle does every new contact complete, and what flux does it link? | Are contact locations and retention reproducible and specifically approved? |
Select the fixing system using separate electrical, mechanical and thermal evidence for the actual assembly. Check furnace exposure, oil compatibility where applicable, retention and coating interaction as distinct requirements.
Verify the path and the retention independently
Retain the before-fixing and after-fixing contact maps. On representative de-energized assemblies, use a qualified inspection and electrical method to verify the intended separation, with the test boundary and acceptance criterion stated. A generic resistance reading between two points on continuous wound strip cannot by itself isolate a local interlaminar bridge; a remote metallic path may already connect the points.
Mechanical verification should establish that the tail remains within its drawing position under the defined manufacturing and handling states. If thermal exposure, curing or fixture release changes the overlap, repeat the inspection in that state. A thermal class or dielectric figure for one component does not prove assembly retention.
Where a changed fixing method needs magnetic validation, compare the relevant loss, excitation and local-temperature evidence under matched operating conditions. The comparison should control core geometry, joints, induction waveform and mechanical restraint. A normal aggregate loss result alone does not demonstrate that every local path is absent.
Release the tail fixing with its overlap geometry, approved material system, closure and contact map. Verify retained position and the intended electrical separation, with every added conductive cycle assessed for its actual linked flux.
Tie the linked-flux screen to a defined steel section
Nippon Steel lists 23ZH90 at a nominal steel thickness of 0.23 mm and an assumed density of 7.65 kg/dm³. [1] Assume a conducting loop links all 100 layers across a 20.0 mm strip width. The linked nominal steel section is 460 mm². At assumed B_pk = 1.5 T and f = 50 Hz, peak flux is 0.000690 Wb and one-turn E_rms is 4.44288 × 50 × 0.000690 = 0.15328 V. A fixing that links only an assumed 5 mm² produces 1.666 mV under the same imposed field, 92 times less. Identify the actual three-dimensional closed path before calculating current or heat. [2]
Manufacturing controls. Control tail overlap, conductor contacts, coating damage, adhesive electrical properties and restraint geometry. Verify retention separately from the test that checks the intended insulation and current paths.
References
[1] Nippon Steel Corporation, Grain-Oriented Electrical Steel Sheets, undated, specification tables and annealing compatibility.
[2] S. Shah et al., Modeling of Losses Due to Inter-Laminar Short-Circuit Currents in Lamination Stacks, 2013, DOI:10.2478/ecce-2013-0012