WEBVTT 00:00:00.452 --> 00:00:02.755 The insulation between laminations is only 00:00:02.770 --> 00:00:04.301 a few microns per side. 00:00:05.155 --> 00:00:07.210 Grain oriented steel normally has a 00:00:07.225 --> 00:00:09.176 glass film and an insulating coating 00:00:09.191 --> 00:00:09.746 above it. 00:00:10.610 --> 00:00:12.640 The outer coating also applies tension 00:00:12.655 --> 00:00:13.418 to the steel. 00:00:14.282 --> 00:00:16.361 Handling can damage both functions. 00:00:17.225 --> 00:00:19.433 Sliding sheets scratches the surface. 00:00:20.285 --> 00:00:22.575 Impacts, bending, hard debris and dull 00:00:22.590 --> 00:00:24.254 cutting edges can crack or remove 00:00:24.269 --> 00:00:24.772 coating. 00:00:25.636 --> 00:00:27.340 If bare areas touch at separate 00:00:27.355 --> 00:00:29.306 points, a conducting loop can form 00:00:29.321 --> 00:00:30.267 between sheets. 00:00:31.105 --> 00:00:33.421 Damaged areas also lose coating tension 00:00:33.436 --> 00:00:34.993 and expose steel to moisture. 00:00:35.858 --> 00:00:37.832 Lift sheets rather than dragging them. 00:00:38.696 --> 00:00:40.345 Keep stacking surfaces clean, 00:00:40.480 --> 00:00:42.405 use suitable lifting aids and maintain 00:00:42.420 --> 00:00:43.314 sharp blades. 00:00:44.165 --> 00:00:45.918 When coating condition is in doubt, 00:00:46.118 --> 00:00:48.421 verify interlaminar resistance using the 00:00:48.436 --> 00:00:49.355 agreed method.