WEBVTT 00:00:00.452 --> 00:00:02.546 Paying for domain-refined steel does not 00:00:02.561 --> 00:00:04.549 guarantee a low-loss finished core. 00:00:05.415 --> 00:00:07.194 Start with the material families: 00:00:07.303 --> 00:00:09.186 conventional grain-oriented steel, 00:00:09.321 --> 00:00:11.715 high-permeability steel, and domain-refined 00:00:11.730 --> 00:00:13.144 high-permeability steel. 00:00:14.009 --> 00:00:16.738 Refinement subdivides the magnetic domains. 00:00:17.590 --> 00:00:19.723 But joints, cutting stress and clamping 00:00:19.738 --> 00:00:21.777 stress still affect the finished core. 00:00:22.642 --> 00:00:24.603 Thinner sheets also change sheet count, 00:00:24.751 --> 00:00:26.582 edge length and the stacking factor. 00:00:27.446 --> 00:00:29.567 Check the complete build before upgrading 00:00:29.582 --> 00:00:30.189 the grade. 00:00:31.040 --> 00:00:32.770 Match the material to the design 00:00:32.785 --> 00:00:34.684 flux density and the agreed loss 00:00:34.699 --> 00:00:35.488 requirement. 00:00:36.340 --> 00:00:38.525 Confirm the intended annealing process is 00:00:38.540 --> 00:00:40.618 compatible with the refinement method. 00:00:41.470 --> 00:00:43.551 Then require a mill certificate traceable 00:00:43.566 --> 00:00:44.212 to the coil, 00:00:44.426 --> 00:00:45.947 and verify that the core builder 00:00:45.962 --> 00:00:47.012 can control joints, 00:00:47.134 --> 00:00:48.249 burrs and stacking.